国产一级特黄aa大片在线-国产一级特黄aa大片免费-国产一级视频在线观看-国产一级视频久久-午夜影院免费体验-午夜影院免费入口

Language:CHINESESENGLISH

Home > News > On the steel building fire scene recognition technology
CONTACT US
  • Address:Pingtang Industrial District, Shipeng Village, Shishan Town, Nanhai District, Foshan City,
  • Phone:0757-81002668/0757-63323396
  • Fax:0757-81196682
  • Contact:Ben Zheng/13826981293 Kerry Lu/13751224830
  • E-mail:sbs@sbsprefabhouse.com
  • URL:http://www.lhp8.cn

On the steel building fire scene recognition technology

Time:[2015-1-31]  Hits:5579

On the steel building fire scene recognition technology

     Steel system with high strength, light weight, low cost, short construction period and other advantages, has been widely used in industrial plants, airports garages, stadiums, shopping centers and other buildings, but the frequency of occurrence of such buildings fire upward trend, especially when there is a major fire occurred. Such as the 1998 Beijing Yuquanying Furniture City Fire Island; August 2003 Taizhou leap AG fire. In the fire scene investigation process, after the building collapsed due to the complexity of the scene, to identify cause of the fire has brought great difficulties.

     Steel at high temperature exhibit unique properties, steel building fire scene is also showing its unique traces of evidence. Through the study of the fire scene steel building components collapse marks, deformation marks, color marks and signs of melting, etc., summarized the effective steel building fire scene recognition technology, for the steel construction of a large fire prone area collapsed, site excavation inquest time-consuming, difficult to determine the fire point the fire site and other issues to provide solutions and technical support.

     Steel is a very important form of civil engineering structures, has been widely used in industrial and civil construction civil engineering. Steel construction including single or low-rise buildings, multi-storey or high-rise buildings, is steel skeleton, with a fire, wall panels and floor waterproof, sound insulation, heat insulation and other features assembled together. Steel is characterized by high strength, low mass; toughness, ductility, high seismic performance; create a simple, short construction period; steel components heat deformation, resulting in the collapse of buildings.

     After the increasing popularity of the use of modern steel, steel building fire and brought the frequency gradually increased, in 1990 the British multi-storey steel building fires occurred during the construction phase, causing steel columns, beams and floor steel severely damaged trusses; September 11, 2001 New York World Trade Center building north and south, respectively, after the hijacked airliner hit the fire, after more than an hour north and south of the burning building have collapsed.

     Studies have shown that the strength of steel decreased with increasing temperature, when the temperature reaches 350 ℃, 500 ℃, 600 ℃, its intensity decreased 1 / 3,1 / 2 and 2/3, respectively; when the temperature exceeds 700 ℃, the component strength To reduce the 80% point easily deformed steel building collapse and so on. In practice, most of the steel building fires often occur in warehouses, barns, shopping malls, and other simple shed, spatial span, doors and windows, good ventilation, combustible materials and more, in case of fire, the fire will be burned more prosperous, in short within the time the fire will develop into a violent stage; this time due to the fire resistance of the steel itself is low, thermal speed again quickly, very short time will be lost in the steel strength, coupled with a lot of steel construction steel components fire Protection is not used, even with a fire retardant coating, because of different quality and price level, some units of investment options to save the poor quality of fire-resistant coating; and a steel body design life is generally 50 years, while the life far fireproof coatings less than 50 years, companies are generally less likely to repaint itself after fire coatings fail, thus resulting in the use late in steel, coated in fire-resistant coating will not achieve the role of fire on it. Also in some steel factories or warehouses, sheds and the like, filling its walls and roof material is often used in polyurethane and polystyrene fire resistance of these two materials is very low, when a fire, often accelerate the temperature dependence of steel components, resulting in a faster component is destroyed, even the collapse of the building and therefore deformed.

     Because executives and super-tall steel building fires small, limited cases, and fires high-rise steel buildings collapse after deformation, live trace feature is not obvious, therefore this paper daily life often occur Strut and large-span steel building fire scene focuses on identifying marks.

     As the inquest collapse marks an important traces of the fire scene evidence, the steel building fires should not be ignored. Formation of collapsed steel building components, a large reason is because the mechanical properties of high-temperature steel external manifestations: Steel stiffness refers to the ability of steel to resist deformation deformation size, stiffness K = EA / L, where E is the elastic modulus amount, A is the cross sectional area, L is the length perpendicular to the cross section. When the fire scene, the cross-sectional area A of its thermal expansion and contraction due to changes in the size of negligible elastic modulus with increasing temperature drastically reduced, resulting in a sharp decrease stiffness K, steel just too small, unable to resist deformation maintain the status quo. Steel fire collapsed and so deformed by instability.

     A basic rule of steel building collapsed traces of fire as a building fire traces, which follows the construction of fire: the fire toward the fire site, or facing the direction of the fire spread to the collapse, but the collapse of the steel structure analysis and certification marks another role different from other fire scene collapse marks, it has its own characteristics. Steel building collapsed into partial collapse and the overall collapse, but no matter what kind of collapse, are part of a part of the collapse, is generally not collapse all at once. After the steel building collapsed in the fire because of their overall connectivity is good, less affected by the fire affect the position change. Xu is now widely used as a building roof trusses are made of non-combustible material made of color steel or galvanized iron, can still save more complete scene after the fire, but unlike timber roof after building fire, by fire and other factors, roof collapse litter larger position changes. Steel roof collapsed building in the shape of the roof of the fire are common U-shaped, beveled shape, and trapezoidal collapse marks.

     Steel roof building fire, if the high fire load within the building, the roof on both sides often appear to form a U-shape facing the collapse of the roof collapsed, which is characterized by both sides of the beams and columns are still together. Bevel-shaped roof collapsed shape is due to a fire in a building close to the side of the formation. After the steel roof building on fire, burned to the site as a result of relying on one side of the building, leading to the connection point of the beams and columns to lose strength, deformation off the formation of the bevel-shaped roof collapsed shape. In multi-span building, if a large area of the roof steel roof collapsed, both parts of the roof collapsed shape bevel shape, another U-shape collapsed, the fire occurred in the U-shaped roof collapsed certainly marks at, because if the first generation of the bevel shaped collapsed shape, indicating that the process of fire spread, the fire burned before the fire across the face of the column cross-share, the share of post and crossbar junction adjacent shedding the first to lose strength under high temperature, and in this case the shape of the roof collapsed under the scarf is certainly not in line with the collapse of the U-shaped features, it should be developed into a U-shaped beveled shape. Trapezoidal shape is usually caused by the collapse of the roof beams or steel roof off the building roof at the side of the seat of the column after the collapse of the scarf did not fall off the side of the fire continued to spread formation.

     Steel building components deform because the strength of steel with the fire temperature increases, the steel in the initial stages of heating, elastic, plastic little change, but at about 250 ℃, the steel tensile strength and impact toughness of the decline this phenomenon is called blue brittle phenomenon (surface oxide film appear blue). When the temperature exceeds 300 ℃ after the yield point and ultimate strength decreased significantly, reaching 500 ℃, which dropped by about half of the original intensity contrast, reach 600 ℃, its strength had declined by two-thirds of contrast. When the steel construction in general the designer, the considered room temperature by a cross-sectional stress under load is half the yield point, and therefore, the temperature rose to 500 ℃, the yield strength decreased to half of the normal temperature, the plastic deformation and damage member to 600 ℃, the strength is almost exhausted. At this point in the dual role of building vertical pressure and horizontal stresses, steel distortion occurs. Since the same coefficient of thermal expansion of steel is not small, the thermal expansion of the fire after the more serious, the steel members at both ends of each surface is restricted or fixed steel member, may also have traces of swelling deformation, the degree of expansion by the same level of influence of temperature, The higher the temperature, the greater the degree of thermal expansion, the greater the deformation.

     Steel building components in fire due to the high temperature effect, its intensity decreases, usually from the fire site closer, its strength relative to other parts of the other parts of the steel components and steel structures, reduced itself more, in the absence of applied load under the circumstances, the performance for the fire deformed downward direction soften, when in the presence of external load situations, the deformed toward the direction of the force. At the same time due to thermal expansion of the role of the degree of thermal expansion of the steel surface by the fire side is larger than the non-face by the fire, the steel members under fire towards the non-plane bending deformation. However, in general the degree of change is less than the degree of thermal expansion due to weakening of the deformation caused.

     In the fire, backfires steel surface under fire first thermal effect, strength decreased, under the premise of no external loads, generally toward the fire point deformation under applied load in the case, toward the direction of the force deformation, which is deformed steel building components acting on the basis of proof marks. By various types of steel buildings and other steel components connected by high strength bolts as a whole, when deformed steel components in a certain part of the scene of the fire by the flame and hot flue gas temperature and other factors, will inevitably bring to the axis of the member local deformation range of building components. With a light steel building basic load-bearing units - portal frame, for example, at the scene of the fire due to the high temperature, the beams and columns are different degrees of deformation, deformation There are two main forms: one-way deformation and deformation tilted toward the middle on both sides. If the fire site near the portal frame columns, steel columns are directly affected by the initial fire flame heat radiation, plastic increased, while the beams by high temperature flue gas rises above 700 ℃, the intensity decreased rapidly; due to their stress, steel door frame beams and columns toward the first heat of the fire point deformation, while the other end of the beam and column far away from the fire site, the role is not affected by temperature, smaller than the decline in the strength of steel, but by pushing the other end of the deformation stress deformation, steel column bent outward to form a one-way tilt deformed steel members; if the fire site is located in the central portal frame, the portal frame this combination, due to temperature effects of fire on both sides of the column is basically the same, and because the suspension hot smoke the role of gas, the first column after losing in the heat carrying capacity of steel beams and tilted toward the fire site, while pulling the sides of the steel beam tilt inward tilt column, the entire steel frame on both sides toward the middle to form a sloping steel components deformation traces its final similar traces shown in Figure 3.5, steel sloping from both sides toward the middle. Throughout the scene of the fire, the fire temperature effect gradually extended over time, initially subjected to high temperature of one or both of the deformed steel frame, steel frame composed of the remaining part of the building at this time of deformation has not occurred, and therefore, deformation of steel and is not deformed steel are drawn by connecting members, generate action and reaction, this form of action, would leave visible marks on the connecting member in the initial fire. The main parts of the two-door is a fire occurred opposite twisted steel steel columns, or near the site of the fire steel connecting member is elongated, pulled off the connection point.

     Steel building components will react with oxygen in the air, the surface oxide layer is formed steel members. Oxidation of the steel greatly affected by temperature, the higher the temperature, the faster the oxidation. Depending on the steel oxidation products under different conditions, the color change of steel, and therefore, there is a correspondence between the traces of steel and oxidation discoloration heating temperature. Steel oxidation reaction occurs much faster than the normal temperature at its surface under fire conditions, produce iron oxide rust layer. If we at high temperatures and in the presence of water or steam to generate part of the role will hydroxide, carbon dioxide in the atmosphere also generates a small amount of basic iron carbonate. When the fire temperature continues to rise by the decomposition of various steel components hydroxide and carbonate material for iron oxide rust. Therefore, the scene of the fire with a fire time and temperature changes, the color of steel components also undergone a series of changes.

     Steel components of different heating temperature and time, the oxide layer formed by different colors. In the scene, in different parts of the steel components, and even the temperature difference is also great on the same components in different parts. Therefore, the color formed on the surface of a significant level, especially the thin-type ferrous metal. Color In general, ferrous metal heat temperature is high, long duration of action of the various parts of the formation showed a red or pale color, color change levels significantly, especially temperature exceeds 800 ℃ portions on its surface also appeared shiny "iron scale "thin, hard and brittle texture. When uncoated steel covered in fire oxidation, the surface becomes dull first blue-gray. Oxidation can be formed thick oxide spalling. After the fire, if the metal has been wet, it can appear usually rusty oxide. On the stainless steel surface, moderate oxidized to form the color pattern, severe oxidation will be formed not shiny gray. Oxidation can form a boundary oxide thickness can show how the size of the fire, heat and processing. The higher the heating temperature, the longer the heating time, the more severe oxidation.

     In the role of fire, steel heating surface will mark oxidation discoloration, mainly iron at high temperature to produce a fire Fe2O3, Fe3O4, FeO, etc., are shown in different colors.

     In different locations and even different steel components due to the different members of the same scene and thus its heat radiation at different temperatures, the surface color is also showing a corresponding different steel building fire can be determined by observing the color change of the steel member hierarchy the fire site. In the actual scene of the fire, the steel components of the color of the surface will show a clear hierarchy, generally fire point as the center outward showing a pale yellow - black and red - blue; some black metal components coated with oil paints, or surface with paint , spray, easy to identify changes in color, but can be burned by the metal surface layer of paint discoloration, cracking, blistering and other changes in level, to identify the temperature change order. And in general we believe that the closer the fire started the fire site, by the time the longer the fire, the temperature will be higher.

     Steel building components melted to form traces in the scene, can be divided into two reasons, first because of the different types of metal components melting point, when the fire temperature reaches the melting point of the metal or melting temperature range, the metal absorbs heat, overcome intermolecular forces, the liquid-solid transition metal melts due to form a melt marks; the second is to produce instant high temperature under the action of the arc, making the metal produce melting traces. Different types of metal, and the relative melting point alloy, at a high temperature under the action of the fire, the metal member is generally difficult to be melted, only a relatively low melting point metal can be melted, such as aluminum and its alloys; However, due to other causes in a short circuit, an arc can leaving traces melt most metals.

     Under fire temperature, steel building components begin to melt the metal is heated to the melting point, the melting temperature of different metals is different, so the scene is formed in accordance with varying degrees of melting traces.

     Temperature continues to rise, reaction time increases, the melting area expanded, the length of the smaller, heavier degree of melting; and for the fire or the fire from spreading in one direction is first heated to melt, the degree of contrast heavier non-heated surface to form a clear the heating surface.

     On the other hand, if the electric arc causes molten metal conductor short-circuited due to the formation of scar, and generally marks the arc formed by molten metal bead and craters on the morphology and melting traces of fire have significantly different: the general arc weld mark for fine columnar crystals or cellular crystal composition, there are holes, one of which was a short circuit inside the pores less melt marks and small, secondary short circuit melt marks are many and large internal pores; and fire places melt marks coarse equiaxed based, almost nonporous.

     Steel building components at the extent of the fire temperature metal melting and temperature effects are intrinsically linked, different metals have different melting points, different degrees of similar metal melting, the site of a large degree of melting temperature is high, and the low melting point and high melting point unmelted molten metal has a high melting point metal explain the higher parts of the temperature. General metal traces by fire after the formation of the temperature effect of light - heavy order: metal surface coating color - blistering - metal surface discoloration - distortion - melted. This marks just the fire and the order corresponding to the temperature changes from low to high order, indicating the direction of fire spread. When the scene of the fire melted the metal structures, the side of the heating temperature for the spread of the direction of the high melting serious fire back surface melting and relatively light. Fire point generally is melted parts, namely, the highest temperature area. This judgment fire all parts of the temperature range and temperature of the fire investigators to provide a scientific basis. If it is found traces the arc melting, melting marks should be further analyzed before the formation of a short circuit or fire fire shorted form, namely a short circuit or shorted secondary. If it is a melting marks, also known as the primary short-circuiting the position is likely to fire point, it is necessary to find the cause of the fire to help the fire point.

     Through research and discussion of this topic, initially found a steel building fire scene traces common feature: the collapse of steel building components, deformation, discoloration, melting and other traces; summarizes the formation mechanism of these traces, through these types of trace evidence steel has been the role of the fire scene is simple, easy to prove the point of the fire or fire spread direction of the fire site approach. When looking for these signs and take advantage of its proven role, always grasp the basic principles of various types of high-temperature fire scene led to the formation of traces of these traces at the mechanical, chemical analysis, and to find the temperature distribution and the steel structure collapsed, deformed correspondence and then indicate the direction for the fire scene investigation.

Copyright:佛山市勝邦鋼結構有限公司 Foshan Shengbang Steel Structure Co., Ltd. Record Number:粵ICP備13078463號
主站蜘蛛池模板: 亿企商贸-亿万企业的商务贸易平台-B2B企业产品发布供求信息平台,一带一路中国企业及产品展示平台,免费企业智能自助建站网络营销推广平台,打造B2B企业黄页产品信息发布推广专业综合电子商务平台! | 阻垢剂|缓蚀剂|杀菌剂|分散剂|水处理剂|印染助剂|水处理药剂|造纸助剂|膜阻垢剂|缓蚀剂|HEDP|ATMP|螯合剂-山东凯瑞化学有限公司 水处理药剂生产厂家 | 塑料托盘 塑料周转箱零件盒生产销售-江苏卡尔富塑业科技有限公司 | 消防施工,消防工程施工,消防施工改造-北京消防工程公司-亿杰(北京)消防工程有限公司 | 洗地机,洗地机价格,扫地机,工业吸尘器,手推式洗地机,驾驶式洗地机,北京洗地机【北京高美环保科技有限公司】 | 造型松|泰山迎客松|造型油松-泰安小苹果园林| 上海便携式液体_日本理音液体_HACH液体颗粒计数器,metone尘埃粒子计数器-上海翰森科学仪器有限公司 | 样品前处理仪器_光谱仪器_色谱/分析仪器_测量/计量仪器_青岛聚创世纪环保科技有限公司 | 中派康明斯发电机_玉柴发电机厂家_静音移动拖车发电机-深圳市斯坦福电力设备有限公司 | 数字多媒体展厅设计,智慧科技互动企业展馆展厅设计公司-深圳炫之风 | 无石棉纤维增强水泥板厂家_水泥纤维装饰板_河北埃尔佳建材科技有限公司 | 销售系统_营销系统_自动营销软件_b2b营销系统_数字营销平台_AI销售 | 长春衡宇机械 食品干燥机 微波灭菌机 连续真空干燥机-干燥行业先进企业 | 铁三角话筒-思美音频处理器-艾伦赫赛数字调音台-北京盛世音盟电子科技有限公司 | 江苏减速机_常州减速机_摆线减速机_摆线针轮减速机 | 联智通达_工控一体机_工业触摸一体机_工业一体机_工业触控一体机_POS机主板_工控主板_国产化主板_RK3588主板厂商-联智通达 | 饮料制造机械设备-罐体设备报价-CIP清洗设备-饮料生产线交钥匙工程-上海哲苏轻工机械有限公司 | 户外工程照明|洗墙灯厂家|聚翔(广东)照明科技有限公司 | 九江中澳钽铌有限公司| 注塑机螺杆_光学无卤耐磨耐腐蚀螺杆_合金材料_螺杆研磨抛光机_杰宇螺杆 | 苏州妙凯电子有限公司-供应军工电源芯片|线性恒流IC|开关电源IC|LED驱动芯片|MOS管|IPM|IGBT|MCU开发|电源模块 | 汽车漆品牌|家具漆代理|涂料加盟厂家|家具漆|汽车漆-邦派漆官网 汽车漆|汽车油漆|工业油漆涂料|汽车漆加盟-佛山市科涂涂料有限公司 | 塑木地板,塑木栏杆,塑木地板价格,塑木地板厂家—浙江尚元塑木制品有限公司 | 塑木地板-木塑地板厂家「云南昆明楚雄曲靖玉溪塑木地板」云南云冶中信塑木新型材料有限公司 | 铁谷网-垂直于铸造产业链服务平台、原材料采购网、行业资讯网 | 金酱酒_金酱酒代理加盟招商_OEM贴牌企业定制! – 金酱酒代理加盟!茅台镇较早的酿酒烧坊,年产优质酱香白酒5000余吨,仁怀市十强白酒企业,主营主品:金酱酒、金酱陈香酒、酱香老酒等系列品牌产品 | 起名字典|宝宝新生儿男孩女孩起名免费网-诗经周易生辰八字取名字大全 | 京建鹏达_商用无烟烧烤设备多少钱|开店商用自助旋转烧烤炉价格|无烟电烧烤炉批发厂家|无烟烧烤桌定做厂商-京建鹏达烧烤设备网 | 汽修学校|汽车维修学校收费|全国职业技校汽修-北京万通汽修学校 汽车轴承|圆锥滚子轴承|轴承生产厂家|赛襄轴承 | 联想南京总代理-联想服务器|联想电脑笔记本代理商|联想工作站|dell服务器|HP服务器|南京IBM代理商|IBM V5000存储总包销-南京宇宽科技有限公司 | 永康微网站建设、永康手机网站建设、永康营销型网站建设、永康外贸网站建设、永康网站托管、永康网络公司—英汇网络 - 永康市英汇网络技术有限公司 | 上海千舟新材料有限公司-美卓隔膜滤板_奥图泰滤板_压滤机配件 | 生物质蒸发器_燃气蒸发器_燃气锅炉价格|厂家直销-山东泰锅锅炉设备有限公司 | 真空烘箱-高低温试验箱-防爆烘箱-防爆高低温试验箱-老化房-恒温恒湿箱-高低温试验箱-高低温冲击试验箱厂家—上海标承实验仪器有限公司 | 贴标机_全自动贴标机_贴标机生产厂家_【佼佼者自动化】 | 正宗舌尖上的卤味卤菜卤肉卤水熟食的做法及配方大全网 | 篮球场围网|网球场围网|球场围网|体育场围网_安平县炎煌丝网制品有限公司 | 小程序商城,_电商系统源码,直播商城定制开发电商系统源码,电商系统,java电商系统 | 学校直饮水机-反渗透纯水设备-家用净水器厂家-广州颖圣能源设备 学校洗碗机-郑州洗碗机厂家-商用洗碗机-郑州旭申环保科技有限公司 | 日本国际高中_上海日本国际高中学校排名_日本国际高中留学课程_上海日语国际高中学校学费-上海工程技术大学国际多语种特色高中课程【官网】 | 著名刑事诉讼律师_刑事辩护律师★王平聚【清华博士/刑法教授】 |